JPH0890191A
|
|
Method for die-casting solid-liquid coexistence in spheroidal graphite cast iron
|
JPH0857587A
|
|
Method for directly forming half-solidified metal slurry
|
JPH0857586A
|
|
Method for casting silicon steel
|
JPH0860267A
|
|
Production of metallic material excellent in workability and method for working the metallic material
|
JPH0852534A
|
|
Continuous casting method of semisolidified metal
|
JPH07214245A
|
|
Production of half solidified metal having excellent workability
|
JPH081281A
|
|
Method and apparatus for producing semi-solidified metallic material
|
JPH07278727A
|
|
Production of high-carbon alloy steel products free from coarse carbide
|
JPH07276036A
|
|
Chilling preventing method in casting of casting iron casting product
|
JPH07256397A
|
|
Manufacture of semi-solidified metal
|
JPH07251242A
|
|
Device for producing half-solidified metal material
|
JPH07251241A
|
|
Device for producing half-solidified metal
|
JPH07216488A
|
|
Al alloy stock for die casting in solid-liquid coexisting region and its production
|
JPH07204783A
|
|
Production of half-solidified metal material having good workability
|
JPH07204820A
|
|
Die casting method for solid-liquid coexisting zone of cast iron
|
JPH07204728A
|
|
Method for extruding solid-liquid coexistent area in metallic material
|
JPH07204729A
|
|
Method for extruding solid-liquid coexistent area in metallic material
|
JPH07155904A
|
|
Device for producing half-solidified metal
|
JPH07155919A
|
|
Method for charging rheometal into die casting machine
|
JPH07155903A
|
|
Device for producing half-solidified metal
|