CS191089A1
|
|
Cooling chamber for toothed wheels' gap induction hardening
|
CS191189A1
|
|
Method of toothed wheels' teeth cooling with module greater than 8 mm
|
CS934187A1
|
|
Method for intermediate roll of sendzimir rolling mill thermal treatment
|
CS120487A1
|
|
Method of primary smoothing-out castings of corrosion-resisting steels
|
CS66587A1
|
|
Method of primary cooling castings made from corrosion-resisting steels
|
CS110386A1
|
|
Method of toothed vheels' surface hardening especially of crown gears
|
CS953285A1
|
|
Method of tools heat treatment especially of tools for sheets and scrap shearing
|
CS265585A1
|
|
Method of treatment of parts subjected to effects of abrasive wear
|
CS548782A1
|
|
Chrome-nickel-molybdenum-tungsten steel for blades cold cutting of plates and steel scrap
|
CS224540B1
|
|
Chrome-mangenese-silicon-vanadium steel,particularly for toothed heels with face hardened teeth being treatened by ionic nitridation
|
CS236959B1
|
|
Chrom-nickel-molybdenum-vanadium steel for blades for cold cutting of super strengh heavy plates
|
CS203821B1
|
|
Process for the surface hardening of toothed wheels having the larger moduls
|